Product description
The main components of fire clay brick k26 fire brick are clay and kaolin, and usually a certain proportion of quartz sand, bauxite, coal gangue and other auxiliary raw materials are added. The content of clay is usually between 50% and 70%, and the content of kaolin is between 10% and 30%.

Applications of k26 fire brick
Power industry: k26 fire brick can be used in power station boiler, flue, desulfurization equipment, dust removal equipment, burner and other high temperature parts.
Construction industry: k26 fire brick can be used for building firewalls, fire doors, flue and other parts.
Other industries: k26 fire brick can also be used in glass, ceramics, petrochemical, mining, machinery manufacturing and other fields.

Physical and chemical index of k26 fire brick
|
Items |
Index |
|
||||||||
|
/ |
N-1 |
N2a |
N2b |
N-3a |
N-3b |
N-4 |
N-5 |
N-6 |
||
|
Refractoriness /℃≥ |
1750 |
1730 |
1730 |
1710 |
1710 |
1690 |
1670 |
1580 |
||
|
0.2Mpa Refractoriness under load(RUL)/℃≥ |
1400 |
1350 |
/ |
1320 |
/ |
1300 |
/ |
/ |
||
|
Reheating linear change/℃(1500℃,2h) |
1400℃,2h |
+0.1 -0.4 |
+0.1 -0.5 |
+0.2 -0.5 |
/ |
/ |
/ |
/ |
/ |
|
|
1350℃,2h |
|
|
|
+0.2 -0.5 |
+0.2 -0.5 |
+0.2 -0.5 |
+0.2 -0.5 |
|
||
|
Apparent porosity/% ≤ |
22 |
24 |
26 |
24 |
26 |
24 |
26 |
28 |
||
|
CCS/Mpa ≥ |
30 |
25 |
20 |
15 |
15 |
20 |
15 |
15 |
||
Packages:

Factory introduction

Zhengzhou Caihua Kiln Masonry Installation Co., Ltd, be called for short of CH Refractories was founded in 1984, have advanced process equipment and raw material preparation system.

A full set of refractories conventional testing equipment, can ensure the quality before sending to customers. Annual production of a variety of shaped and unshaped refractory materials 120,000 tons.

CH Refractories mainly produce refractory materials for metallurgical, coking, cement industry, electric power industry, chemical and general industrial furnaces. The refractory products exported to Middle east, South America, Middle Asia, Southeast Asia, Africa and other regions.
FAQ
Q: What is Foreign Trade-Express?
Q: How can I get price at soonest?
Q: Can I get sample for testing?
Q: What is MOQ of your product?
Q: How can you guarantee your products quality
Q: Which countries you mainly exporting to?
Q: How long is the production time?
Q: What payment term you can accept?
Q: Can you do OEM? Or customized packages?
Q: Can I visit your factory?
Physical and chemical index of k26 fire brick
|
Items |
Index |
|
||||||||
|
/ |
N-1 |
N2a |
N2b |
N-3a |
N-3b |
N-4 |
N-5 |
N-6 |
||
|
Refractoriness /℃≥ |
1750 |
1730 |
1730 |
1710 |
1710 |
1690 |
1670 |
1580 |
||
|
0.2Mpa Refractoriness under load(RUL)/℃≥ |
1400 |
1350 |
/ |
1320 |
/ |
1300 |
/ |
/ |
||
|
Reheating linear change/℃(1500℃,2h) |
1400℃,2h |
+0.1 -0.4 |
+0.1 -0.5 |
+0.2 -0.5 |
/ |
/ |
/ |
/ |
/ |
|
|
1350℃,2h |
|
|
|
+0.2 -0.5 |
+0.2 -0.5 |
+0.2 -0.5 |
+0.2 -0.5 |
|
||
|
Apparent porosity/% ≤ |
22 |
24 |
26 |
24 |
26 |
24 |
26 |
28 |
||
|
CCS/Mpa ≥ |
30 |
25 |
20 |
15 |
15 |
20 |
15 |
15 |
||